Cylindrical specimens (6 mm high x 4 mm diameter) of the endodontic grade glass-ionomer (Ketac Endo) were exposed to various media for 1 week, after which changes in their mass, pH of storage medium, and ion release were determined. In water, this cement was shown to release reasonable amounts of sodium, aluminium and silicon, together with smaller amounts of calcium and phosphorus, as well as taking up 2.41% by mass of water. A comparison with the restorative grade materials (Ketac Molar, ex 3M ESPE and Fuji IX, ex GC) showed both ion release and water uptake to be greater. All three cements shifted pH from 7 to around 6 with no significant differences between them. Other storage media were found to alter the pattern of ion release. Lactic acid caused an increase, whereas both saturated calcium hydroxide and 0.6% sodium hypochlorite, caused decreases. This suppression of ion-release may be significant clinically. Aluminium is the most potentially hazardous of the ions involved but amounts released were low compared with levels previously reported to show biological damage.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objectives. To evaluate the response of the pulpo-dentin complex following application of a resin-modified glass-ionomer cement or an adhesive system in deep cavities performed in human teeth.Methods. Deep class V cavities were prepared on the buccal surface of 26 premolars. In Group I the cavity walls (dentin) and enamel were conditioned with 32% phosphoric acid and the dentin adhesive system One Step (Bisco, Inc., Itasca, IL, USA) was applied. In Groups 2 and 3, before total etching and application of bonding agent, the cavity floor was lined with the resin-modified glass-ionomer cement-Vitrebond (3M ESPE Dental Products Division, St. Paul, MN, USA) or the calcium hydroxide cement-Dycal (control group, Dentsply, Mildford, DE, USA), respectively. The cavities were restored using light-cured Z-100 composite resin (3M ESPE). The teeth were extracted between 5 and 30 days and prepared for microscopic assessment. Serial sections were stained with H/E, Masson's trichrome, and Brown and Brenn techniques.Results. In Group 1, the inflammatory response was more evident than in Groups 2 and 3. Diffusion of dental material components across dentinal tubules was observed only in Group 1, in which the intensity of the pulp response increased as the remaining dentin thickness decreased. Bacteria were evidenced in the lateral walls of two samples (Group 2) which exhibited no inflammatory response or tissue disorganization.Conclusions. Based on the experimental conditions, it was concluded total acid etching followed by application of One Step bonding agent cannot be recommended as adequate procedures. In this clinical condition the cavity walls should be lined with a biocompatible dental material, such as Vitrebond or Dycal. 2003 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: Ultrasonic excitation (US) was applied to glass ionomer cement (GIC) during early set time to increase the advantageous properties of this material. Purpose: The aim of this in vitro study was to assess the inner porosity of GIC after US. Study design: A total of 16 specimens, for each material, were prepared from high-viscosity GIC Fuji IX GP, Ketac Molar, and Ketac Molar Easymix. Half of these specimens (n = 8) received 30 s of US during the initial cement setting. After completion of the material setting, specimens were fractured and observed by scanning electronic microscopy to quantitatively assay porosity inside the material using Image J software. Results: Statistical data analysis revealed that US reduced the porosity for all tested materials (P <= 0.05). The following reductions (expressed in percentages) were achieved: Fuji IX-from 3.9% to 2.8%; Ketac Molar Easy Mix-from 4.4% to 2.6%, and Ketac Molar-from 2.4% to 1.6%. Conclusion: Under the tested conditions, US was an effective method for porosity reduction inside the material. Microsc. Res. Tech. 74:54-57, 2011. (C) 2010 Wiley-Liss, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this study was to evaluate the presence of porosities inside the glass ionomer cement (GIC) after different techniques of material insertion. MATERIAL and METHOD: Specimens were prepared with high-viscosity GIC Ketac Molar Easymix and divided into three groups according to the insertion method: spatula (PI), Centrix injector (CI), and low-cost syringe (LCS). The specimens were fractured and observed with scanning electronic microscopy to quantitatively evaluate porosity inside the material using Image J Software. RESULTS: Statistical analysis, ANOVA application, and Tukey test to significance level of 5%, revealed that there was no statistical difference between the groups. CONCLUSION: Although the use of LCS has not decreased the porosity of the material, this insertion method is easy, accessible, and low cost, which makes it a viable alternative of use in the ART technique and in others bucal health programs. Microsc. Res. Tech., 2012. (c) 2012 Wiley Periodicals, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: to evaluate the human pulp response following pulp capping with calcium hydroxide (CI-I, Group 1), and the resin-modified glass-ionomer Vitrebond (VIT, Group 2). Materials and Methods: Intact teeth with no cavity preparation were used as control Group (ICG, Group 3). Buccal Class V cavities were prepared in 34 sound human premolars. After exposing the pulps, the pulp capping materials were applied and the cavities were Filled using Clearfil Liner Bond 2 bonding agent and Z100 resin-based composite. The teeth were extracted after 5, 30, and from 120 to 300 days, fixed in 10% buffered formalin solution, and prepared according to routine histological techniques. 6-mu m sections were stained with hematoxylin and eosin, Masson's trichrome, or Brown gr Brenn technique for bacterial observation. Results: At 5 days, CH caused a large zone of coagulation necrosis, the mononuclear inflammatory reaction underneath the necrotic zone was slight to moderate. VIT caused a moderate to intense inflammatory pulp response with a large necrotic zone. A number of congested venules associated with plasma extravasation and neutrophilic infiltration was observed. Over time, only CH allowed pulp repair and complete dentin bridging around the pulp exposure site. VIT components displaced into the pulp tissue triggered a persistent inflammatory reaction which appeared to be associated with a lack of dentin bridge formation. After 30 days a few histological sections showed a number of bacteria on the lateral dentin walls. In these samples the pulp response was similar to those samples with no microleakage. VIT was more irritating to pulp tissue than CH, which allowed pulp repair associated with dentin bridge formation. These results suggested that VIT is not an appropriate dental material to be used in direct pulp capping for mechanically exposed human pulps.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this paper is to compare the fluoride-releasing and mechanical properties of an experimental luting glass ionomer cement, which has a modified composition and a commercial luting cement. The experimental powder was obtained by sol-gel process and then, it was used to prepare the experimental cements. The properties of cement pastes, such as setting time and working time, microhardness and diametral tensile strength were determined. Fluoride release from GICs was evaluated at time intervals of 1, 7, 14, 21 and 28 days in deionized water. Atomic force microscopy (AFM) analyses showed that the surface of the experimental cements is more homogeneous than commercial GICs. The mechanical properties and the measure of liberation of fluoride of the two cements were influenced by ratio powder:liquid and chemical composition of the precursor powders. Experimental cements released less fluoride than commercial cements. However, this liberation was more constant during the analyzed period. Thus, the results obtained in this study indicated that the composition of the experimental powder modified by the niobium can lead the formation of the polysalt matrix with good mechanical properties. In other words, we can say that experimental powder offered considerable promise for exploitation in dental field.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Glass ionomer cements (GICs) are currently used for various dental applications such as luting cements or as restorative materials. The calcium fluoro-alumino-silicate system is the basis for degradable glasses used to obtain the GICs. The purpose of the present paper is to add niobium to conventional glass system because according to previous papers niobium addition improves the chemical resistance and the mechanical properties of glasses. Therefore, the GICs prepared from these glasses would result in cements with higher chemical and mechanical resistance. The niobium fluoride powders were prepared using the sol-gel process and were characterized by X-ray diffraction, differential thermal analysis (DTA) and Al-27 and Si-29 MAS NMR. The results obtained by XRD showed that the powders prepared by this method are glass-ceramic. In the DTA curve was detected the presence of T-g and T-c temperatures. The analysis of MAS NMR spectra indicated that the framework of the powders is formed by SiO4 and AlO4 linked tetrahedra which are essential structures to yield the cements. Thus, we concluded that niobium fluoride silicate powders can be used in the preparation of GICs. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this in vitro study was to evaluate the effect of different bur types and acid etching protocols on the shear bond strength (SBS) of a resin modified glass ionomer cement (RM-GIC) to primary dentin. Forty-eight clinically sound human primary molars were selected and randomly assigned to four groups (n=12). In G1, the lingual surface of the teeth was cut with a carbide bur until a 2.0-mm-diameter dentin area was exposed, followed by the application of RM-GIC (Vitremer - 3M/ESPE) prepared according to the manufacturer's instructions. The specimens of G2, received the same treatment of G1, however the dentin was conditioned with phosphoric acid. In groups G3 and G4 the same procedures of G1 and G2 were conducted respectively, nevertheless dentin cutting was made with a diamond bur. The specimens were stored in distilled water at 37 degrees C for 24h, and then tested in a universal testing machine. SBS. data were submitted to 2-way ANOVA (= 5%) and indicated that SBS values of RM-GIC bonded to primary dentin cut with different burs were not statistically different, but the specimens that were conditioned with phosphoric acid presented SBS values significantly higher that those without conditioning. To observe micromorphologic characteristics of the effects of dentin surface cut by diamond or carbide rotary instruments and conditioners treatment, some specimens were examined by scanning electron microscopy. Smear layer was present in all specimens regardless of the type of rotary instrument used for dentin cutting, and specimens etched with phosphoric acid presented more effective removal of smear layer. It was concluded that SBS of a RM-GIC to primary dentin was affected by the acid conditioning but the bur type had no influence.